Equivalents · Q355B vs S355J2

Q355B vs S355J2

These two grades are listed as equivalents of each other: their chemistry windows overlap and they serve the same applications. They are not always identical — check the differences below before substituting, especially in certified designs.

Q355B

Structural & HSLA Steel

Q355B is the current GB/T 1591 designation that replaced Q345B in the 2018 revision, with the yield class raised from 345 to 355 MPa to align with international S355 practice. It is now the standard Chinese HSLA for structures, machinery and pipe.

Standards: DIN S355J2 (near) · AISI A572 Gr.50 (near) · JIS SM490B (near) · GB Q355B (GB/T 1591)

S355J2

Pipe & Tube Steel

S355J2 is Europe’s structural HSLA steel (EN 10025-2), the benchmark for welded structures, machinery and pipe where −20 °C toughness is specified.

Standards: DIN 1.0577 (S355J2) / 1.0570 legacy St52-3 · AISI A572 Gr.50 (near) · JIS SM490B (near) · GB Q345B (near)

Chemical composition compared (%)

ElementQ355BS355J2
C≤0.24≤0.20
Si≤0.55≤0.55
Mn≤1.60≤1.60
P≤0.035≤0.025
S≤0.035≤0.025

Properties compared

PropertyQ355BS355J2
Yield strength≥355 MPa (≤16 mm)≥355 MPa (≤16 mm)
Tensile strength470–630 MPa470–630 MPa
ImpactB grade: 34 J at 20 °CJ2: −20 °C, ≥27 J
Density7.85 g/cm³7.85 g/cm³

Sourcing either grade?

Nasteel stocks both families from Shenzhen with EN 10204 3.1 mill certificates by heat number.

Ask for a quotation

See full data sheets: Q355B · S355J2. Substitution decisions for certified parts stay with the design authority.