Equivalents · 1141 vs 1144

1141 vs 1144

These two grades are listed as equivalents of each other: their chemistry windows overlap and they serve the same applications. They are not always identical — check the differences below before substituting, especially in certified designs.

1141

Carbon Steel

1141 pairs 1040-class carbon with 1.35–1.65% manganese and resulfurization, giving free-machining bar with better hardenability than 1140. It is a popular cold drawn grade for machined shafts and studs.

Standards: AISI 1141

1144

Carbon Steel

1144 is a heavily resulfurized, high manganese carbon steel that reaches high strength in the as-drawn condition while machining freely. In North America it is sold under trade names for stress-proof-type shafting applications (trademark names belong to their owners).

Standards: AISI 1144

Chemical composition compared (%)

Element11411144
C0.37–0.450.40–0.48
Mn1.35–1.651.35–1.65
P≤0.040≤0.040
S0.08–0.130.24–0.33

Properties compared

Property11411144
Tensile strength560–670 MPa (hot rolled, typ.)660–780 MPa (hot rolled, typ.)
Density7.85 g/cm³7.85 g/cm³
Yield strength—≥410 MPa (typ.)

Sourcing either grade?

Nasteel stocks both families from Shenzhen with EN 10204 3.1 mill certificates by heat number.

Ask for a quotation

See full data sheets: 1141 · 1144. Substitution decisions for certified parts stay with the design authority.