430

Stainless Steel

430 is the most widely used ferritic stainless steel, a 17% chromium, nickel-free grade with good corrosion resistance in mild atmospheres and excellent resistance to nitric acid. It is the standard grade for appliance trim and decorative sheet.

Standards: DIN 1.4016 · AISI 430 · JIS SUS430 · GB 10Cr17

439

Stainless Steel

439 is a stabilised 17–19% chromium ferritic stainless with low carbon and nitrogen, giving better formability, weldability and corrosion resistance than 430. It is used for exhaust systems and heat-exchanger tubing as a lower-cost alternative to 304.

Standards: DIN 1.4510 · AISI 439 · GB 06Cr17Ti

Chemical composition compared (%)

Element430439
C≤0.12≤0.03
Si≤1.00≤1.00
Mn≤1.00≤1.00
P≤0.040≤0.040
S≤0.030≤0.030
Cr16.00–18.0017.00–19.00
Ni≤0.75≤0.50
Ti—0.20+4×(C+N)–1.10
N—≤0.03

Properties compared

Property430439
Delivery conditionAnnealedAnnealed
Hardness≤183 HB (annealed)≤183 HB (annealed)
Tensile strength450–600 MPa415–585 MPa
Yield strength≥205 MPa—
Density7.70 g/cm³7.70 g/cm³
MagneticYesYes

Sourcing either grade?

Nasteel stocks both families from Shenzhen with EN 10204 3.1 mill certificates by heat number.

Ask for a quotation

See full data sheets: 430 · 439. Substitution decisions for certified parts stay with the design authority.