Equivalents · API K55 Casing vs API N80 Casing

API K55 Casing vs API N80 Casing

These two grades are listed as equivalents of each other: their chemistry windows overlap and they serve the same applications. They are not always identical — check the differences below before substituting, especially in certified designs.

API K55 Casing

Pipe & Tube Steel

K55 sits one step above J55 in the API 5CT casing ladder: the same yield window but a higher minimum tensile strength (655 vs 517 MPa), bought with a slightly richer mill chemistry that API still leaves to the producer. It is the default step-up for deeper or higher-load strings.

Standards: AISI API 5CT K55 · GB K55 (GB/T 19830)

API N80 Casing

Pipe & Tube Steel

N80 is the mid-strength API 5CT casing and tubing grade for deeper wells beyond J55/K55 capability. Type Q (Q&T) is preferred where collapse resistance and uniform properties matter.

Standards: AISI API 5CT N80 (Type 1 / Q) · GB N80 (GB/T 19830)

Chemical composition compared (%)

ElementAPI K55 CasingAPI N80 Casing
P≤0.030≤0.030
S≤0.030≤0.030
NoteAPI 5CT sets no C/Mn limits for K55 — chemistry is mill practiceType Q is quenched & tempered; Type 1 normalized — chemistry is mill practice

Properties compared

PropertyAPI K55 CasingAPI N80 Casing
Yield strength379–552 MPa (55–80 ksi)552–758 MPa (80–110 ksi)
Tensile strength≥655 MPa (95 ksi)≥689 MPa (100 ksi)
Density7.85 g/cm³7.85 g/cm³

Sourcing either grade?

Nasteel stocks both families from Shenzhen with EN 10204 3.1 mill certificates by heat number.

Ask for a quotation

See full data sheets: API K55 Casing · API N80 Casing. Substitution decisions for certified parts stay with the design authority.