Equivalents · 9255 vs 9260

9255 vs 9260

These two grades are listed as equivalents of each other: their chemistry windows overlap and they serve the same applications. They are not always identical — check the differences below before substituting, especially in certified designs.

9255

Alloy & Engineering Steel

9255 is a Si-Cr spring steel combining the sag resistance of silicon with chromium hardenability. It serves coil and leaf springs that are too thick for plain Si-Mn grades to harden through.

Standards: DIN 1.5026 (55Si7 family, near) · AISI 9255 · JIS SUP7 (near) · GB 55Si2Mn (near)

9260

Alloy & Engineering Steel

9260 is a silicon-manganese spring steel with about 2% silicon, giving an exceptionally high yield-to-tensile ratio and resistance to permanent set (sag). It is a mainstream coil spring steel for vehicle suspensions.

Standards: DIN 1.5028 (65Si7 family, near) · AISI 9260 · JIS SUP6 (near) · GB 60Si2Mn (near)

Chemical composition compared (%)

Element92559260
C0.51–0.590.56–0.64
Si1.20–1.601.80–2.20
Mn0.70–0.900.75–1.00
Cr0.70–0.90—
P≤0.035≤0.035
S≤0.040≤0.040

Properties compared

Property92559260
Hardness (spring temper)40–48 HRC typical40–50 HRC typical
Tensile strength1200–1500 MPa (Q&T spring temper, typ.)1300–1600 MPa (Q&T spring temper, typ.)
Density7.85 g/cm³7.85 g/cm³

Sourcing either grade?

Nasteel stocks both families from Shenzhen with EN 10204 3.1 mill certificates by heat number.

Ask for a quotation

See full data sheets: 9255 · 9260. Substitution decisions for certified parts stay with the design authority.