Equivalents · 4720 vs 8620

4720 vs 8620

These two grades are listed as equivalents of each other: their chemistry windows overlap and they serve the same applications. They are not always identical — check the differences below before substituting, especially in certified designs.

4720

Alloy & Engineering Steel

4720 is a mid-nickel Ni-Cr-Mo carburizing steel between 8620 and 4320 in cost and core toughness. It serves medium-duty gears that outgrow 8620 but do not justify full 4320 alloy content.

Standards: AISI 4720

8620

Alloy & Engineering Steel

8620 is the standard carburizing (case-hardening) gear steel of the Americas: a low-carbon Ni-Cr-Mo grade that forms a hard wear-resistant case over a tough core.

Standards: DIN 1.6523 (21NiCrMo2-2) · AISI 8620 · JIS SNCM220 · GB 20CrNiMo

Chemical composition compared (%)

Element47208620
C0.19–0.240.18–0.23
Si0.15–0.350.15–0.35
Mn0.50–0.700.70–0.90
P≤0.035—
S≤0.040—
Cr0.35–0.550.40–0.60
Ni0.90–1.200.40–0.70
Mo0.15–0.250.15–0.25

Properties compared

Property47208620
Case hardness (carburized)58–62 HRC58–63 HRC
Core tensile strength700–950 MPa (typ.)—
Density7.85 g/cm³7.85 g/cm³
Core tensile—700–950 MPa

Sourcing either grade?

Nasteel stocks both families from Shenzhen with EN 10204 3.1 mill certificates by heat number.

Ask for a quotation

See full data sheets: 4720 · 8620. Substitution decisions for certified parts stay with the design authority.