U75V

Structural & HSLA Steel

U75V is China’s vanadium-microalloyed rail steel to GB/T 2585, the workhorse upgrade over U71Mn for busy passenger and freight lines. Higher carbon, silicon and a small vanadium addition lift as-rolled strength to the 980 MPa class and slow head wear and rolling-contact fatigue.

Standards: DIN R350HT class (near, EN 13674) · GB U75V (GB/T 2585)

U71Mn

Structural & HSLA Steel

U71Mn is China’s standard carbon rail steel to GB/T 2585, the pearlitic C-Mn grade laid on most conventional-speed lines. Wear resistance comes from its high carbon and manganese; weldability is limited and rail joints are aluminothermic or flash-butt welded.

Standards: DIN R260 family (near, EN 13674) · GB U71Mn (GB/T 2585)

Chemical composition compared (%)

ElementU75VU71Mn
C0.71–0.800.65–0.76
Si0.50–0.800.15–0.35
Mn0.70–1.051.10–1.40
V0.04–0.12—
P≤0.030≤0.030
S≤0.030≤0.030

Properties compared

PropertyU75VU71Mn
Tensile strength≥980 MPa (as-rolled rail)≥880 MPa (as-rolled rail)
Hardness~280–320 HB (rail head, typ.)~260–300 HB (rail head, typ.)
Density7.85 g/cm³7.85 g/cm³

Sourcing either grade?

Nasteel stocks both families from Shenzhen with EN 10204 3.1 mill certificates by heat number.

Ask for a quotation

See full data sheets: U75V · U71Mn. Substitution decisions for certified parts stay with the design authority.