Equivalents · DH40 vs EH40

DH40 vs EH40

These two grades are listed as equivalents of each other: their chemistry windows overlap and they serve the same applications. They are not always identical — check the differences below before substituting, especially in certified designs.

DH40

Structural & HSLA Steel

DH40 pairs the 390 MPa strength of the 40-series hull steels with impact toughness certified at −20 °C. It is specified for hull zones and vessel types that see cold water or winter service, where AH40’s 0 °C guarantee is not enough.

Standards: AISI A131 DH40 · JIS KD40 (near) · GB DH40 (GB/T 712)

EH40

Structural & HSLA Steel

EH40 is the arctic member of the 390 MPa hull-steel family: same chemistry window as AH40/DH40, but impact-certified at −40 °C. Ice-classed vessels, Arctic offshore units and cold-climate port structures are its home ground.

Standards: AISI A131 EH40 · JIS KE40 (near) · GB EH40 (GB/T 712)

Chemical composition compared (%)

ElementDH40EH40
C≤0.18≤0.18
Si≤0.50≤0.50
Mn0.90–1.600.90–1.60
P≤0.035≤0.035
S≤0.035≤0.035
NoteNb/V/Ti grain-refining per class rulesNb/V/Ti grain-refining per class rules

Properties compared

PropertyDH40EH40
Yield strength≥390 MPa≥390 MPa
Tensile strength510–660 MPa510–660 MPa
Impact−20 °C, ≥41 J longitudinal (≤50 mm)−40 °C, ≥41 J longitudinal (≤50 mm)
Density7.85 g/cm³7.85 g/cm³

Sourcing either grade?

Nasteel stocks both families from Shenzhen with EN 10204 3.1 mill certificates by heat number.

Ask for a quotation

See full data sheets: DH40 · EH40. Substitution decisions for certified parts stay with the design authority.