Equivalents · M36 vs M35

M36 vs M35

These two grades are listed as equivalents of each other: their chemistry windows overlap and they serve the same applications. They are not always identical — check the differences below before substituting, especially in certified designs.

M36

Tool Steel

M36 applies the 8% cobalt treatment to the M2 base composition, giving red hardness close to M42 with a slightly different carbide balance. It is an older American cobalt grade still specified for heavy cutting tools.

Standards: AISI M36 · GB W6Mo5Cr4V2Co8 (near)

M35

Tool Steel

M35 is M2 with about 5% cobalt added, the most popular cobalt high-speed steel worldwide. The cobalt raises red hardness so tools keep cutting at the higher speeds and feeds used on stainless and alloy steels.

Standards: DIN 1.3243 · AISI M35 · JIS SKH55 · GB W6Mo5Cr4V2Co5

Chemical composition compared (%)

ElementM36M35
C0.80–0.900.87–0.95
Si≤0.45≤0.45
Mn≤0.40≤0.40
Cr3.75–4.503.75–4.50
Mo4.50–5.504.70–5.20
W5.50–6.505.90–6.70
V1.75–2.251.70–2.10
Co7.75–8.754.50–5.00

Properties compared

PropertyM36M35
Delivery conditionAnnealedAnnealed
Hardness (hardened)63–66 HRC63–66 HRC
Density8.10 g/cm³8.10 g/cm³
Red hardnessHigh (8% cobalt)Higher than M2 (5% cobalt)

Sourcing either grade?

Nasteel stocks both families from Shenzhen with EN 10204 3.1 mill certificates by heat number.

Ask for a quotation

See full data sheets: M36 · M35. Substitution decisions for certified parts stay with the design authority.