Equivalents · A8 vs A2

A8 vs A2

These two grades are listed as equivalents of each other: their chemistry windows overlap and they serve the same applications. They are not always identical — check the differences below before substituting, especially in certified designs.

A8

Tool Steel

A8 is an air-hardening 5% chromium cold work steel with tungsten and molybdenum, positioned between A2 and the hot work family. Its secondary-hardening response suits cold work tools that run warm, such as extrusion backers and warm-heading dies.

Standards: AISI A8

A2

Tool Steel

A2 is an air-hardening 5% chromium cold work steel with much better toughness than D2 and far less distortion than oil-hardening grades. It is the default upgrade from O1 where die size or intricate shapes make quench cracking a risk.

Standards: DIN 1.2363 · AISI A2 · JIS SKD12 · GB Cr5Mo1V

Chemical composition compared (%)

ElementA8A2
C0.50–0.600.95–1.05
Si0.75–1.100.10–0.50
Mn0.20–0.500.40–1.00
Cr4.75–5.254.75–5.50
Mo1.15–1.650.90–1.40
W2.00–2.50—
V—0.15–0.50

Properties compared

PropertyA8A2
Delivery conditionAnnealedAnnealed
Hardness (hardened)52–58 HRC57–62 HRC
Density7.85 g/cm³7.85 g/cm³
Toughness—Good for cold work

Sourcing either grade?

Nasteel stocks both families from Shenzhen with EN 10204 3.1 mill certificates by heat number.

Ask for a quotation