Equivalents · A2 vs D2

A2 vs D2

These two grades are listed as equivalents of each other: their chemistry windows overlap and they serve the same applications. They are not always identical — check the differences below before substituting, especially in certified designs.

A2

Tool Steel

A2 is an air-hardening 5% chromium cold work steel with much better toughness than D2 and far less distortion than oil-hardening grades. It is the default upgrade from O1 where die size or intricate shapes make quench cracking a risk.

Standards: DIN 1.2363 · AISI A2 · JIS SKD12 · GB Cr5Mo1V

D2

Tool Steel

D2 is the world-standard high-carbon, high-chromium cold work tool steel. Massive chromium carbides give exceptional abrasive wear resistance and long die life in blanking and forming.

Standards: DIN 1.2379 · AISI D2 · JIS SKD11 · GB Cr12Mo1V1

Chemical composition compared (%)

ElementA2D2
C0.95–1.051.45–1.60
Si0.10–0.500.10–0.60
Mn0.40–1.000.20–0.60
Cr4.75–5.5011.00–13.00
Mo0.90–1.400.70–1.00
V0.15–0.500.70–1.00

Properties compared

PropertyA2D2
Delivery conditionAnnealedAnnealed
Hardness (hardened)57–62 HRC58–62 HRC
Density7.85 g/cm³7.70 g/cm³
ToughnessGood for cold work—
Wear resistance—Very high

Sourcing either grade?

Nasteel stocks both families from Shenzhen with EN 10204 3.1 mill certificates by heat number.

Ask for a quotation