Equivalents · API C90 Casing vs API T95 Casing

API C90 Casing vs API T95 Casing

These two grades are listed as equivalents of each other: their chemistry windows overlap and they serve the same applications. They are not always identical — check the differences below before substituting, especially in certified designs.

API C90 Casing

Pipe & Tube Steel

C90 is a controlled-hardness API 5CT grade for sour (H₂S) wells: quenched-and-tempered to a 90 ksi yield window while the hardness is capped at 25.4 HRC so sulfide stress cracking cannot start. It is specified where N80-type material would be an SSC risk.

Standards: AISI API 5CT C90 · GB C90 (GB/T 19830)

API T95 Casing

Pipe & Tube Steel

T95 is the stronger sibling of C90 in the API 5CT sour-service family: 95 ksi yield with the same 25.4 HRC hardness ceiling and sulfide-stress-cracking test regime. It serves deep sour wells where C90’s strength runs out but P110-class hardness would be an SSC hazard.

Standards: AISI API 5CT T95 · GB T95 (GB/T 19830)

Chemical composition compared (%)

ElementAPI C90 CasingAPI T95 Casing
P≤0.030≤0.030
S≤0.030≤0.030
NoteAPI 5CT controls C90 by strength, hardness and SSC testing — no C/Mn composition limitsAPI 5CT controls T95 by strength, hardness and SSC testing — no C/Mn composition limits

Properties compared

PropertyAPI C90 CasingAPI T95 Casing
Yield strength621–758 MPa (90–105 ksi)655–758 MPa (95–110 ksi)
Tensile strength≥689 MPa (100 ksi)≥724 MPa (105 ksi)
Hardness≤25.4 HRC (sour-service cap)≤25.4 HRC (sour-service cap)
Density7.85 g/cm³7.85 g/cm³

Sourcing either grade?

Nasteel stocks both families from Shenzhen with EN 10204 3.1 mill certificates by heat number.

Ask for a quotation

See full data sheets: API C90 Casing · API T95 Casing. Substitution decisions for certified parts stay with the design authority.