Equivalents · SKD11 vs D2

SKD11 vs D2

These two grades are listed as equivalents of each other: their chemistry windows overlap and they serve the same applications. They are not always identical — check the differences below before substituting, especially in certified designs.

SKD11

Tool Steel

SKD11 is the JIS cold work tool steel equivalent to AISI D2 and DIN 1.2379 — the Asian-market designation buyers meet on Japanese and Korean mill certificates.

Standards: DIN 1.2379 · AISI D2 · JIS SKD11 · GB Cr12Mo1V1

D2

Tool Steel

D2 is the world-standard high-carbon, high-chromium cold work tool steel. Massive chromium carbides give exceptional abrasive wear resistance and long die life in blanking and forming.

Standards: DIN 1.2379 · AISI D2 · JIS SKD11 · GB Cr12Mo1V1

Chemical composition compared (%)

ElementSKD11D2
C1.40–1.601.45–1.60
Si≤0.400.10–0.60
Mn≤0.600.20–0.60
Cr11.00–13.0011.00–13.00
Mo0.80–1.200.70–1.00
V0.20–0.500.70–1.00

Properties compared

PropertySKD11D2
Delivery conditionAnnealedAnnealed
Hardness (hardened)58–62 HRC58–62 HRC
Density7.70 g/cm³7.70 g/cm³
Wear resistance—Very high

Sourcing either grade?

Nasteel stocks both families from Shenzhen with EN 10204 3.1 mill certificates by heat number.

Ask for a quotation

See full data sheets: SKD11 · D2. Substitution decisions for certified parts stay with the design authority.