Equivalents · API 2H Gr.50 vs S355J2

API 2H Gr.50 vs S355J2

These two grades are listed as equivalents of each other: their chemistry windows overlap and they serve the same applications. They are not always identical — check the differences below before substituting, especially in certified designs.

API 2H Gr.50

Structural & HSLA Steel

API 2H Grade 50 is the offshore-structure plate specification: a normalized, fine-grain C-Mn steel with 345 MPa yield, −40 °C Charpy toughness and a capped carbon equivalent, written for welded jackets, decks and nodes that must survive North-Sea-class fatigue and low temperatures. Supplementary through-thickness (Z) and CTOD requirements are commonly invoked on top of the base spec.

Standards: DIN — (cf. EN 10225 S355G offshore grades) · AISI API 2H Gr.50

S355J2

Pipe & Tube Steel

S355J2 is Europe’s structural HSLA steel (EN 10025-2), the benchmark for welded structures, machinery and pipe where −20 °C toughness is specified.

Standards: DIN 1.0577 (S355J2) / 1.0570 legacy St52-3 · AISI A572 Gr.50 (near) · JIS SM490B (near) · GB Q345B (near)

Chemical composition compared (%)

ElementAPI 2H Gr.50S355J2
C≤0.18≤0.20
Si0.05–0.50≤0.55
Mn1.15–1.60≤1.60
P≤0.030≤0.025
S≤0.010≤0.025

Properties compared

PropertyAPI 2H Gr.50S355J2
Yield strength≥345 MPa≥355 MPa (≤16 mm)
Tensile strength483–620 MPa470–630 MPa
Impact≥41 J at −40 °C (transverse)J2: −20 °C, ≥27 J
Carbon equivalentCE(IIW) ≤0.43 typical spec cap—
Density7.85 g/cm³7.85 g/cm³

Sourcing either grade?

Nasteel stocks both families from Shenzhen with EN 10204 3.1 mill certificates by heat number.

Ask for a quotation

See full data sheets: API 2H Gr.50 · S355J2. Substitution decisions for certified parts stay with the design authority.