Equivalents · 1524 vs 1541

1524 vs 1541

These two grades are listed as equivalents of each other: their chemistry windows overlap and they serve the same applications. They are not always identical — check the differences below before substituting, especially in certified designs.

1524

Carbon Steel

1524 is a low carbon steel with 1.35–1.65% manganese, giving noticeably better hardenability and core strength than 1020/1022. It is a cost-effective carburizing steel for larger case-hardened parts.

Standards: AISI 1524 · GB 20Mn (near)

1541

Carbon Steel

1541 upgrades 1040-class carbon with high manganese, the cheapest way to buy hardenability in a plain steel. It is widely used for axles, shafts and bolts in North American bar programs.

Standards: AISI 1541 · JIS SMn438 family (near) · GB 40Mn (near)

Chemical composition compared (%)

Element15241541
C0.19–0.250.36–0.44
Mn1.35–1.651.35–1.65
P≤0.040≤0.040
S≤0.050≤0.050

Properties compared

Property15241541
Tensile strength440–540 MPa (hot rolled, typ.)600–720 MPa (normalized, typ.)
Density7.85 g/cm³7.85 g/cm³

Sourcing either grade?

Nasteel stocks both families from Shenzhen with EN 10204 3.1 mill certificates by heat number.

Ask for a quotation

See full data sheets: 1524 · 1541. Substitution decisions for certified parts stay with the design authority.