Equivalents · R350HT vs R260

R350HT vs R260

These two grades are listed as equivalents of each other: their chemistry windows overlap and they serve the same applications. They are not always identical — check the differences below before substituting, especially in certified designs.

R350HT

Structural & HSLA Steel

R350HT is the heat-treated premium rail grade of EN 13674-1. In-line head hardening refines the pearlitic microstructure, pushing head hardness to 350–390 HBW and tensile strength above 1175 MPa — the standard answer for heavy-haul lines, sharp curves and high-tonnage metro systems where R260 wears too fast.

Standards: DIN R350HT (EN 13674-1) · GB U75V (near, GB/T 2585)

R260

Structural & HSLA Steel

R260 is the world’s standard rail steel grade to EN 13674-1, a pearlitic carbon-manganese steel whose as-rolled head hardness of 260–300 HBW balances wear against weldability and cost. Most conventional and mixed-traffic lines outside China are laid in R260.

Standards: DIN R260 (EN 13674-1) · GB U71Mn (near, GB/T 2585)

Chemical composition compared (%)

ElementR350HTR260
C0.70–0.820.62–0.80
Si0.15–0.580.15–0.58
Mn0.65–1.250.65–1.25
P≤0.020≤0.025
S≤0.025≤0.025
Cr≤0.30≤0.15

Properties compared

PropertyR350HTR260
Tensile strength≥1175 MPa (rail)≥880 MPa (rail, as-rolled)
Hardness350–390 HBW (rail head)260–300 HBW (rail head)
Density7.85 g/cm³7.85 g/cm³

Sourcing either grade?

Nasteel stocks both families from Shenzhen with EN 10204 3.1 mill certificates by heat number.

Ask for a quotation

See full data sheets: R350HT · R260. Substitution decisions for certified parts stay with the design authority.