Equivalents · SKD11 vs D3

SKD11 vs D3

These two grades are listed as equivalents of each other: their chemistry windows overlap and they serve the same applications. They are not always identical — check the differences below before substituting, especially in certified designs.

SKD11

Tool Steel

SKD11 is the JIS cold work tool steel equivalent to AISI D2 and DIN 1.2379 — the Asian-market designation buyers meet on Japanese and Korean mill certificates.

Standards: DIN 1.2379 · AISI D2 · JIS SKD11 · GB Cr12Mo1V1

D3

Tool Steel

D3 is an ultra-high-carbon chromium steel with even more carbide than D2 and no Mo/V additions. It maximizes abrasive wear life at the lowest cost, but with the lowest toughness of the D-family.

Standards: DIN 1.2080 · AISI D3 · JIS SKD1 · GB Cr12

Chemical composition compared (%)

ElementSKD11D3
C1.40–1.601.90–2.20
Si≤0.400.10–0.60
Mn≤0.600.20–0.60
Cr11.00–13.0011.00–13.00
Mo0.80–1.20—
V0.20–0.50—

Properties compared

PropertySKD11D3
Delivery conditionAnnealedAnnealed
Hardness (hardened)58–62 HRC58–64 HRC
Density7.70 g/cm³7.70 g/cm³
Wear resistance—Extreme (abrasive)

Sourcing either grade?

Nasteel stocks both families from Shenzhen with EN 10204 3.1 mill certificates by heat number.

Ask for a quotation

See full data sheets: SKD11 · D3. Substitution decisions for certified parts stay with the design authority.