Equivalents · EH36 vs DH36

EH36 vs DH36

These two grades are listed as equivalents of each other: their chemistry windows overlap and they serve the same applications. They are not always identical — check the differences below before substituting, especially in certified designs.

EH36

Structural & HSLA Steel

EH36 is the premium 355 MPa hull grade with impact toughness guaranteed at −40 °C — standard for LNG/LPG carriers, ice-going ships and Arctic offshore structures. It is the toughest of the widely traded 36-series ship plate.

Standards: AISI A131 EH36 · JIS KE36 (near) · GB EH36 (GB/T 712)

DH36

Structural & HSLA Steel

DH36 is the −20 °C impact version of the 355 MPa hull grade, specified for vessels trading in cold waters and for exposed structure where AH36 toughness is insufficient. Chemistry is the same family as AH36; the difference is the toughness guarantee and its verification.

Standards: AISI A131 DH36 · JIS KD36 (near) · GB DH36 (GB/T 712)

Chemical composition compared (%)

ElementEH36DH36
C≤0.18≤0.18
Si≤0.50≤0.50
Mn0.90–1.600.90–1.60
P≤0.035≤0.035
S≤0.035≤0.035
NoteNb/V/Ti grain-refining per class rulesNb/V/Ti grain-refining per class rules

Properties compared

PropertyEH36DH36
Yield strength≥355 MPa≥355 MPa
Tensile strength490–630 MPa490–630 MPa
Impact−40 °C, ≥34 J longitudinal (≤50 mm)−20 °C, ≥34 J longitudinal (≤50 mm)
Density7.85 g/cm³7.85 g/cm³

Sourcing either grade?

Nasteel stocks both families from Shenzhen with EN 10204 3.1 mill certificates by heat number.

Ask for a quotation

See full data sheets: EH36 · DH36. Substitution decisions for certified parts stay with the design authority.