Equivalents · 1215 vs 1117

1215 vs 1117

These two grades are listed as equivalents of each other: their chemistry windows overlap and they serve the same applications. They are not always identical — check the differences below before substituting, especially in certified designs.

1215

Carbon Steel

1215 is a rephosphorized and resulfurized free-cutting steel with very low carbon, built purely for machining speed. It is one of the fastest-cutting bar steels available and a staple of high-volume screw machining.

Standards: AISI 1215 · JIS SUM25 (near) · GB Y12 (near)

1117

Carbon Steel

1117 is a resulfurized free-machining steel: added sulfur and high manganese give fast, clean cutting while keeping enough carbon to carburize. It is a standard screw-machine grade for small turned parts in volume.

Standards: AISI 1117 · JIS SUM family (near) · GB Y15 (near)

Chemical composition compared (%)

Element12151117
C≤0.090.14–0.20
Mn0.75–1.051.00–1.30
P0.04–0.09≤0.040
S0.26–0.350.08–0.13

Properties compared

Property12151117
Tensile strength380–460 MPa (hot rolled, typ.)400–480 MPa (hot rolled, typ.)
Machinability≈135% of 1212 (typ. rating)≈90% of 1212 (typ. rating)
Density7.85 g/cm³7.85 g/cm³

Sourcing either grade?

Nasteel stocks both families from Shenzhen with EN 10204 3.1 mill certificates by heat number.

Ask for a quotation

See full data sheets: 1215 · 1117. Substitution decisions for certified parts stay with the design authority.