Equivalents · 12L14 vs 1215

12L14 vs 1215

These two grades are listed as equivalents of each other: their chemistry windows overlap and they serve the same applications. They are not always identical — check the differences below before substituting, especially in certified designs.

12L14

Carbon Steel

12L14 is the leaded free-cutting steel: lead, sulfur and phosphorus together give the highest machinability of any standard bar steel. It dominates high-volume turned parts where cycle time rules, at the cost of weldability and environmental restrictions on lead.

Standards: DIN 11SMnPb30 family (near) · AISI 12L14 · JIS SUM24L (near) · GB Y12Pb (near)

1215

Carbon Steel

1215 is a rephosphorized and resulfurized free-cutting steel with very low carbon, built purely for machining speed. It is one of the fastest-cutting bar steels available and a staple of high-volume screw machining.

Standards: AISI 1215 · JIS SUM25 (near) · GB Y12 (near)

Chemical composition compared (%)

Element12L141215
C≤0.15≤0.09
Mn0.85–1.150.75–1.05
P0.04–0.090.04–0.09
S0.26–0.350.26–0.35
Pb0.15–0.35—

Properties compared

Property12L141215
Tensile strength390–470 MPa (hot rolled, typ.)380–460 MPa (hot rolled, typ.)
Machinability≈160–170% of 1212 (typ. rating)≈135% of 1212 (typ. rating)
Density7.85 g/cm³7.85 g/cm³

Sourcing either grade?

Nasteel stocks both families from Shenzhen with EN 10204 3.1 mill certificates by heat number.

Ask for a quotation

See full data sheets: 12L14 · 1215. Substitution decisions for certified parts stay with the design authority.