A572 Gr.55

Structural & HSLA Steel

ASTM A572 Grade 55 is a columbium-vanadium HSLA structural steel one step above the ubiquitous Gr.50: yield rises to ≥380 MPa (55 ksi) and tensile to ≥485 MPa (70 ksi) while chemistry stays lean and weldable. It is used where Gr.50 sections become too heavy but Gr.65 hardenability is not wanted.

Standards: DIN S355J2 (near) · AISI A572 Gr.55 · JIS SM490B (near) · GB Q355B (near)

A572 Gr.50

Structural & HSLA Steel

ASTM A572 Grade 50 is the standard American HSLA structural steel — the 50 ksi yield grade that replaced A36 in most US bridge and heavy construction work. Strength comes from Nb/V microalloying and grain refinement rather than carbon, so weldability remains good.

Standards: DIN S355J2 (near) · AISI A572 Gr.50 · JIS SM520B (near) · GB Q355B (near)

Chemical composition compared (%)

ElementA572 Gr.55A572 Gr.50
C≤0.25≤0.23
Si≤0.40≤0.40
Mn≤1.35≤1.35
P≤0.04≤0.035
S≤0.05≤0.045
NoteStrength comes from a Nb, V or Nb-V addition — Type 1, 2, 3 or 5 must be specified on the order—
V—0.01–0.15 (Type 2)

Properties compared

PropertyA572 Gr.55A572 Gr.50
Yield strength≥380 MPa≥345 MPa
Tensile strength≥485 MPa≥450 MPa
Density7.85 g/cm³7.85 g/cm³

Sourcing either grade?

Nasteel stocks both families from Shenzhen with EN 10204 3.1 mill certificates by heat number.